Thermal Properties Metric English Comments
Thermal Conductivity 154 W/m-K
1070 BTU-in/hr-ft²-°F
Aleris Hokotol Aluminum Alloy, 200 mm Thickness
Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an..
Thermal Conductivity 154 W/m-K
1070 BTU-in/hr-ft²-°F
Aleris Hokotol Aluminum Alloy, 100 mm Thickness
Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an..
Thermal Conductivity 154 W/m-K
1070 BTU-in/hr-ft²-°F
Aleris Hokotol Aluminum Alloy, 300 mm Thickness
Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an..
Thermal Conductivity 154 W/m-K
1070 BTU-in/hr-ft²-°F
Aleris Hokotol Aluminum Alloy, 325 mm Thickness
Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an..