Thermal Properties Metric English Comments
Thermal Conductivity 22.2 W/m-K

@Temperature 700 °C
154 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes HR-120® alloy, solution heat-treated
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 22.2 W/m-K

@Temperature 700 °C
154 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 22.2 W/m-K

@Temperature 700 °C
154 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 22.2 W/m-K

@Temperature 700 °C
154 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 22.2 W/m-K

@Temperature 700 °C
154 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 22.2 W/m-K

@Temperature 700 °C
154 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 718 alloy, cold rolled, solution-treated and aged sheet
Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i..