Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 10.9 - 23.0 W/m-K @Temperature 150 - 150 °C |
75.6 - 160 BTU-in/hr-ft²-°F @Temperature 302 - 302 °F |
Average value: 17.0 W/m-K Grade Count:1 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Thermal Conductivity | 10.9 - 23.0 W/m-K @Time 3600 - 3600 sec |
75.6 - 160 BTU-in/hr-ft²-°F @Time 1.00 - 1.00 hour |
Average value: 17.0 W/m-K Grade Count:1 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |