Thermal Properties Metric English Comments
Thermal Conductivity 23.96 W/m-K

@Temperature 300 °C
166.3 BTU-in/hr-ft²-°F

@Temperature 572 °F
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel
CPM REX M4 HC(HS) is a high vanadium special purpose high speed steel exhibiting better wear resistance and toughness than M2 or M3 in cold work punches, die inserts and cutting applications involvi..