Polymer Property : Thermal Conductivity = 17.31 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 17.31 W/m-K

@Temperature 93.0 °C
120.1 BTU-in/hr-ft²-°F

@Temperature 199 °F
Crucible Steel CPM® S30V® Stainless Steel
CPM S30V is a martensitic stainless steel designed to offer the best combination of toughness, wear resistance and corrosion resistance. Its chemistry has been specially balanced to promote the form..
Thermal Conductivity 17.31 W/m-K

@Temperature 93.0 °C
120.1 BTU-in/hr-ft²-°F

@Temperature 199 °F
Crucible Steel CPM® S35VN™ Stainless Steel
CPM S35VN is a martensitic stainless steel designed to offer improved toughness over CPM S30V. It is also easier to machine and polish than CPM S30V. Its chemistry has been rebalanced so that it for..