Thermal Properties Metric English Comments
Thermal Conductivity 18.07 W/m-K

@Temperature 500 °C
125.4 BTU-in/hr-ft²-°F

@Temperature 932 °F
ATI Wah Chang Tiadyne™ 3510
Capable of being surface hardened to depths that produce very high wear resistance. Produced by traditional metallurgical processing, not special treatments.Information provided by ATI Wah Chang