Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.09 W/m-K @Temperature 540 °C |
181.1 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel CPM REX M4 HC(HS) is a high vanadium special purpose high speed steel exhibiting better wear resistance and toughness than M2 or M3 in cold work punches, die inserts and cutting applications involvi.. |