Thermal Conductivity 183 W/m-K
1270 BTU-in/hr-ft²-°F
CMW® 353 Copper Alloy
CMW® 353 material is an economical high strength, high conductivity copper base alloy. It is a heat treatable copper base alloy and its excellent properties are obtained largely through heat treatm..