Thermal Properties Metric English Comments
Thermal Conductivity 270 - 280 W/m-K
1870 - 1940 BTU-in/hr-ft²-°F
x-y direction
MarkeTech Cu/Mo/Cu 1:2:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..