Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.306 W/m-K | 2.12 BTU-in/hr-ft²-°F | ASTM F433 |
Sumitomo Bakelite North America 52-20-30 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Thermal Conductivity | 0.305 W/m-K | 2.12 BTU-in/hr-ft²-°F | |
Cytec EN-2543 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Thermal Conductivity | 0.306 W/m-K | 2.12 BTU-in/hr-ft²-°F | Melt |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |