Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.349 W/m-K | 2.41 BTU-in/hr-ft²-°F | |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Thermal Conductivity | 0.349 W/m-K | 2.41 BTU-in/hr-ft²-°F | |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |