Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.398 W/m-K | 2.76 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Bond 862-7 General Purpose Epoxy Adhesive TRA-BOND 862-7 semi-flexible, nonflowing epoxy paste adhesive is designed for general purpose applications. It is suitable for bonding materials with mismatched coefficients of expansion. This epoxy.. |