Thermal Properties Metric English Comments
Thermal Conductivity 0.428 W/m-K
2.97 BTU-in/hr-ft²-°F
ASTM E-1925-06
Haysite SDL® H400 Polyester Composite
H400 is an advanced composite that combines high temperature resistant and high strength characteristics with static dissipative properties for use as wave and reflow solder pallets. SDL Grade H400..