Polymer Property : Thermal Conductivity = 20.3 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 538°C (1000°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 704°C (1300°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, welded and tested as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, weld metal as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, weld metal, aged 500 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 20.3 W/m-K
141 BTU-in/hr-ft²-°F
Special Metals UDIMET® Alloy 250 Maraging Steel
A high-strength, maraging steel of iron and nickel with additions of molybdenum and titanium. It has the strength of standard 18Ni (250) maraging steel but the advantages of containing less molybde..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 593°C (1100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 760°C (1400°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, 1.6 mm sheet, aged 128 hours at 815°C (1500°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 20.3 W/m-K

@Temperature 600 °C
141 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® N, 1.14 mm sheet, heat treated at 1149°C (2100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Special Metals INCOLOY® Alloy 903
A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a..