Thermal Properties Metric English Comments
Thermal Conductivity 21.4 W/m-K

@Temperature 600 °C
149 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
Thermal Conductivity 21.4 W/m-K

@Temperature 700 °C
149 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 800 °C
149 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 700 °C
149 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 800 °C
149 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 700 °C
149 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 800 °C
149 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 700 °C
149 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 800 °C
149 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 700 °C
149 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 800 °C
149 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 700 °C
149 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 800 °C
149 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 21.4 W/m-K

@Temperature 700 °C
149 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..
Thermal Conductivity 21.4 W/m-K

@Temperature 800 °C
149 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..