Thermal Properties Metric English Comments
Thermal Conductivity 3.22 W/m-K
22.3 BTU-in/hr-ft²-°F
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive
EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go..