Polymer Property : Thermal Conductivity = 228 W/m-K
Polymer Property :
Thermal Conductivity =
228 W/m-K
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Thermal Conductivity
228
W/m-K
1580
BTU-in/hr-ft²-°F
Goodfellow Tungsten 60/Copper 40 Alloy
Information provided by Goodfellow.