Polymer Property : Thermal Conductivity = 244 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 35.2 W/m-K
244 BTU-in/hr-ft²-°F
DIN EN 821-2 / ASTM-C408
CeramTec 614/698 Alumina, 96%
614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink.