Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.60 W/m-K @Temperature 800 °C |
25.0 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
McDanel Advanced Ceramics MV-30 Mullite Information provided by McDanel Advanced Ceramic Technologies |
|||
Thermal Conductivity | 3.60 W/m-K | 25.0 BTU-in/hr-ft²-°F | |
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy Description: Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring high thermal conductivity, excellent electrical insulation properties and N.. |
|||
Thermal Conductivity | 3.60 W/m-K | 25.0 BTU-in/hr-ft²-°F | |
Master Bond Supreme 11AN Two Component, Heat Resistant Epoxy Adhesive Description: Master Bond Polymer Adhesive System Supreme 11AN is a two component thermally conductive heat resistant epoxy adhesive with a one-to-one mix ratio, by weight or volume. It readily devel.. |
|||
Thermal Conductivity | 3.60 W/m-K | 25.0 BTU-in/hr-ft²-°F | |
Cotronics Duralco™ 127 400°F (200°C) Graphite Filled Epoxy One component, graphite filled epoxy for low cost production applications. Can be used with automatic dispensing equipment. |