Thermal Properties Metric English Comments
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 27.5 W/m-K
191 BTU-in/hr-ft²-°F
ASTM-C408
CoorsTek CAP 4 98.5% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Thermal Conductivity 27.5 W/m-K
191 BTU-in/hr-ft²-°F
ASTM-C408
CoorsTek FG-98 98% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Thermal Conductivity 27.5 W/m-K
191 BTU-in/hr-ft²-°F
ASTM C408
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Thermal Conductivity 27.5 W/m-K

@Temperature 1000 °C
191 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..