Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 39.0 W/m-K @Temperature 85.0 °C |
271 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 13 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Thermal Conductivity | 39.0 W/m-K @Temperature 215 °C |
271 BTU-in/hr-ft²-°F @Temperature 419 °F |
ASTM E457 |
3D Systems LaserForm™ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing Parts fabricated from this rapid prototype metal material are actually a blend of stainless steel and bronze. The part is built with steel and subsequently infiltrated with bronze. A6 is great for .. |