Polymer Property : Thermal Conductivity = 275 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 275 W/m-K
1910 BTU-in/hr-ft²-°F
(x-y)
GrafTech GRAFCELL® FFP-100 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
Thermal Conductivity 275 W/m-K
1910 BTU-in/hr-ft²-°F
(x-y)
GrafTech GRAFCELL® FFP-200 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
Thermal Conductivity 275 W/m-K
1910 BTU-in/hr-ft²-°F
(x-y)
GrafTech GRAFCELL® FFP-300 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
Thermal Conductivity 275 W/m-K
1910 BTU-in/hr-ft²-°F
Ametek Molybdenum-Copper Composite AMC 3169
Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng..