Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 28.5 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 28.5 W/m-K

@Temperature 1000 °C
198 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
Thermal Conductivity 28.5 W/m-K

@Temperature 95.0 °C
198 BTU-in/hr-ft²-°F

@Temperature 203 °F
Crucible Steel S7 (AISI S7) Tool Steel
Crucible S7 is a shock resisting tool steel with excellent toughness and high strength, along with low to medium wear resistance. It has been widely used for many years to make chisels and punches w..
Thermal Conductivity 28.5 W/m-K

@Temperature 95.0 °C
198 BTU-in/hr-ft²-°F

@Temperature 203 °F
Crucible Steel S7 XL (Premium AISI S7) Tool Steel
Crucible S7XL is a double refined, high purity grade of S7. The remelt operation produces a cleaner steel with a more uniform microstructure, offering the following advantages over conventional S7:B..
Thermal Conductivity 28.5 W/m-K
198 BTU-in/hr-ft²-°F
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7)
TLS S7 Shock-Resisting tool steel is an air or oil hardening tool steel that is characterized by very high impact toughness. The combination of strength and high toughness makes S7 tool steel a cand..
Copyright © lookpolymers.com All Rights Reserved