Polymer Property : Thermal Conductivity = 3.30 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 3.30 W/m-K

@Temperature 800 °C
22.9 BTU-in/hr-ft²-°F

@Temperature 1470 °F
McDanel Advanced Ceramics MV-20 Mullite
Information provided by McDanel Advanced Ceramic Technologies
Thermal Conductivity 3.30 W/m-K
22.9 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® ED1021 Epoxy
Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Unique features include its abil..