Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.39 W/m-K @Temperature 20.0 - 800 °C |
23.5 BTU-in/hr-ft²-°F @Temperature 68.0 - 1470 °F |
|
Corning Pyroceram® Glass Ceramic High strength, high elastic modulus, and uniform dielectric properties. Pyroceram® can be manufactured in ogival ( pointed arch) shapes, hemispheres, pressware sheets, and various machined shapes. .. |