Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.40 W/m-K | 23.6 BTU-in/hr-ft²-°F | Nominal, Through-Plane; ASTM-D5470 Modified Method |
GrafTech eGRAF® SPREADERSHIELD™ SS1500 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thermal Conductivity | 3.40 W/m-K | 23.6 BTU-in/hr-ft²-°F | |
Du-Co Ceramics CS-144-L-5 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Thermal Conductivity | 3.40 W/m-K | 23.6 BTU-in/hr-ft²-°F | |
Du-Co Ceramics DC-10-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Thermal Conductivity | 3.40 W/m-K | 23.6 BTU-in/hr-ft²-°F | |
Du-Co Ceramics DC-16-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Thermal Conductivity | 3.40 W/m-K | 23.6 BTU-in/hr-ft²-°F | |
Du-Co Ceramics DC-65 Cordierite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Thermal Conductivity | 3.40 W/m-K | 23.6 BTU-in/hr-ft²-°F | |
Du-Co Ceramics DC-9-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Thermal Conductivity | 3.40 W/m-K @Pressure 30.0 MPa, Temperature 50.0 °C |
23.6 BTU-in/hr-ft²-°F @Pressure 4350 psi, Temperature 122 °F |
Product Property; Arlon SQA-TMS-054 |
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |