Polymer Property : Thermal Conductivity = 3.54 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
ASTM E1225
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer
Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
Quadrant EPP Semitron® MPR-1000 (ASTM Product Data Sheet)
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 1-RG 2 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 1/CF/30/TF/13/SI/2/BK Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 1/CF/30/TF/15 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S..
Thermal Conductivity 0.510 W/m-K

@Temperature 100 °C
3.54 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007..
Thermal Conductivity 0.510 W/m-K

@Temperature 100 °C
3.54 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 4349 Phenolic, Granular, Compression Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..
Thermal Conductivity 0.510 W/m-K

@Temperature 100 °C
3.54 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 5488 Phenolic, Granular, Injection Molded
PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not ..
Thermal Conductivity 0.510 W/m-K

@Temperature 100 °C
3.54 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 4002 Phenolic, Granular, Injection Molded
PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
ASTM C177
Unitika UNILATE® 1 PC PET
Standard gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and othe..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
ASTM E1461
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound
Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
ASTM E1225
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser..
Thermal Conductivity 0.510 W/m-K
3.54 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical ..
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 100 - 100 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.570 W/m-K Grade Count:4
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..