Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 322 W/m-K | 2230 BTU-in/hr-ft²-°F | |
OMG Americas GlidCop® AL-60 Dispersion Strengthened Copper GlidCop® AL-60 is copper that is dispersion strengthened with 1.1 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum o.. |
|||
Thermal Conductivity | 322 W/m-K | 2230 BTU-in/hr-ft²-°F | |
CMW® 328 Copper Alloy CMW® 328 material is a high strength, high conductivity copper base alloy. CMW® 328 is heat treatable. Optimum mechanical and physical properties of CMW® 328 material are developed by heat treatm.. |