Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 46.8 W/m-K @Temperature 10.0 - 232 °C |
325 BTU-in/hr-ft²-°F @Temperature 50.0 - 450 °F |
|
Meehanite GC-40 Flake Graphite Cast Iron Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake d.. |