Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 34.5 W/m-K @Temperature 95.0 °C |
239 BTU-in/hr-ft²-°F @Temperature 203 °F |
|
Crucible Steel HALGRAPH® Tool Steel, AISI O6 Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a.. |
|||
Thermal Conductivity | 34.5 W/m-K @Temperature 95.0 °C |
239 BTU-in/hr-ft²-°F @Temperature 203 °F |
|
Crucible Steel KETOS® Tool Steel, AISI O1 Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording.. |