Thermal Conductivity 359.7 W/m-K
2496 BTU-in/hr-ft²-°F
Eagle Brass 151 ZHC® COPPER, 1/2 Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Thermal Conductivity 359.7 W/m-K
2496 BTU-in/hr-ft²-°F
Eagle Brass 151 ZHC® COPPER, 1/4 Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Thermal Conductivity 359.7 W/m-K
2496 BTU-in/hr-ft²-°F
Eagle Brass 151 ZHC® COPPER, 3/4 Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Thermal Conductivity 359.7 W/m-K
2496 BTU-in/hr-ft²-°F
Eagle Brass 151 ZHC® COPPER, Annealed
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Thermal Conductivity 359.7 W/m-K
2496 BTU-in/hr-ft²-°F
Eagle Brass 151 ZHC® COPPER, Extra Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Thermal Conductivity 359.7 W/m-K
2496 BTU-in/hr-ft²-°F
Eagle Brass 151 ZHC® COPPER, Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Thermal Conductivity 359.7 W/m-K
2496 BTU-in/hr-ft²-°F
Eagle Brass 151 ZHC® COPPER, Spring
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Thermal Conductivity 359.7 W/m-K
2496 BTU-in/hr-ft²-°F
Cadi 162 Copper Alloy
Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium..