Polymer Property : Thermal Conductivity = 37.49 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 37.49 W/m-K
260.2 BTU-in/hr-ft²-°F
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel
LESCALLOY 300M-HS VAC-ARC steel is a modified 4340 steel with added silicon allowing for use of a higher tempering temperature. The steel has high hardenability and strength with good ductility and ..
Thermal Conductivity 37.49 W/m-K
260.2 BTU-in/hr-ft²-°F
Latrobe Lescalloy® 300M VAC-ARC High Strength Alloy Steel
LESCALLOY 300M VAC-ARC steel is a modified 4340 steel with added silicon allowing for use of a higher tempering temperature. The steel has high hardenability and strength with good ductility and tou..
Thermal Conductivity 37.49 W/m-K
260.2 BTU-in/hr-ft²-°F
Latrobe Lescalloy® HY-TUF VAC-ARC High Strength Alloy Steel
LESCALLOY HY-TUF VAC-ARC steel is a high strength low alloy steel. It is typically used in the 220/240 ksi (1517/1655 MPa) tensile strength range. At this strength level, the alloy has good ductilit..