Thermal Properties Metric English Comments
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
MMCC Al/Al2O3 Particulate Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
Parallel to pressing direction
Momentive Performance Materials HBR Hot-Pressed Boron Nitride
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom..
Thermal Conductivity 55.0 - 125 W/m-K

@Temperature 2300 °C
382 - 868 BTU-in/hr-ft²-°F

@Temperature 4170 °F
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder
A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u..
Thermal Conductivity 55.0 - 125 W/m-K

@Temperature 2300 °C
382 - 868 BTU-in/hr-ft²-°F

@Temperature 4170 °F
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder
Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder ..
Thermal Conductivity 55.0 - 125 W/m-K

@Temperature 2300 °C
382 - 868 BTU-in/hr-ft²-°F

@Temperature 4170 °F
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder
A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u..
Thermal Conductivity 55.0 - 125 W/m-K

@Temperature 2300 °C
382 - 868 BTU-in/hr-ft²-°F

@Temperature 4170 °F
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder
Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced..
Thermal Conductivity 55.0 - 125 W/m-K

@Temperature 2300 °C
382 - 868 BTU-in/hr-ft²-°F

@Temperature 4170 °F
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder
Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TD2 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TDX Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TH1 Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TH1 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TH2 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TH3 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TH4 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 THX Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 THX Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TD1 Rod quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TD1 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TD3 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
CLAL-MSX DECLAFOR® 1015 TF Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..