Polymer Property : Thermal Conductivity = 4.21 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.607 W/m-K
4.21 BTU-in/hr-ft²-°F
ASTM F433
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy
Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc.