Thermal Properties Metric English Comments
Thermal Conductivity 0.620 W/m-K
4.30 BTU-in/hr-ft²-°F
Schott SF57 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.620 W/m-K
4.30 BTU-in/hr-ft²-°F
Schott SF57HHT Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.620 W/m-K

@Temperature 100 °C
4.30 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 3356 Phenolic, Granular, Compression Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
Thermal Conductivity 0.620 W/m-K
4.30 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Algoflon® 35CAR PTFE; Petroleum Coke and Graphite  (discontinued **)
Data provided by the manufacturer.35 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p..
Thermal Conductivity 0.620 W/m-K
4.30 BTU-in/hr-ft²-°F
C518/C177
Saint-Gobain Meldin® 2021 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..
Thermal Conductivity 0.620 W/m-K
4.30 BTU-in/hr-ft²-°F
Ceradyne Thermo-Sil® Castable 120 Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..
Thermal Conductivity 0.620 W/m-K
4.30 BTU-in/hr-ft²-°F
Ceradyne Thermo-Sil® Castable TG Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..