Polymer Property : Thermal Conductivity = 59.5 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 8.57 W/m-K
59.5 BTU-in/hr-ft²-°F
in-plane, ø80*3mm discs; ISO 22007-2
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6
LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive.
Thermal Conductivity 8.57 W/m-K
59.5 BTU-in/hr-ft²-°F
in-plane, ø80*3mm discs; ISO 22007-2
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 compound
Thermal Conductivity 8.57 W/m-K
59.5 BTU-in/hr-ft²-°F
in-plane, ø80*3mm discs; ISO 22007-2
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral filled PA6 compound