Thermal Properties Metric English Comments
Thermal Conductivity 6.10 W/m-K
42.3 BTU-in/hr-ft²-°F
ASTM E-1461
Ovation Polymers Nemcon™ H PC DP105/X3 BK Polycarbonate
Polycarbonate-Black colored, thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers