Thermal Properties Metric English Comments
Thermal Conductivity 0.908 W/m-K
6.30 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Ketron® CM 1030HT PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products
Thermal Conductivity 0.908 W/m-K
6.30 BTU-in/hr-ft²-°F
ASTM C177
Quantum PEEK 30% Carbon Filled
Information provided by Quantum Advanced Engineering Plastics
Thermal Conductivity 0.908 W/m-K
6.30 BTU-in/hr-ft²-°F
Schott N-LAK9 Glass
Information Provided by SCHOTT North America, Inc.