Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0600 - 6.50 W/m-K | 0.416 - 45.1 BTU-in/hr-ft²-°F | Average value: 1.09 W/m-K Grade Count:59 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |