Polymer Property : Thermal Conductivity = 624 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 89.9 W/m-K
624 BTU-in/hr-ft²-°F
Ohio Carbon Blank OCB AR-12 EDM Grade Graphite
Available in a range of sizes and shapes.
Thermal Conductivity 89.9 W/m-K
624 BTU-in/hr-ft²-°F
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Thermal Conductivity 89.9 W/m-K
624 BTU-in/hr-ft²-°F
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Thermal Conductivity 89.9 W/m-K
624 BTU-in/hr-ft²-°F
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Thermal Conductivity 89.9 W/m-K
624 BTU-in/hr-ft²-°F
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Thermal Conductivity 89.9 W/m-K
624 BTU-in/hr-ft²-°F
Materion BrushCAST® 275CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Thermal Conductivity 89.9 W/m-K
624 BTU-in/hr-ft²-°F
Materion BrushCAST® 275C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..