Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 100 W/m-K | 696 BTU-in/hr-ft²-°F | |
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Thermal Conductivity | 100 W/m-K | 696 BTU-in/hr-ft²-°F | |
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Thermal Conductivity | 100 W/m-K | 696 BTU-in/hr-ft²-°F | |
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Thermal Conductivity | 100 W/m-K | 696 BTU-in/hr-ft²-°F | |
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Thermal Conductivity | 100 W/m-K | 696 BTU-in/hr-ft²-°F | |
Materion BrushCAST® 165CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Thermal Conductivity | 100 W/m-K | 696 BTU-in/hr-ft²-°F | |
Materion BrushCAST® 165C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |