Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.03 W/m-K | 7.15 BTU-in/hr-ft²-°F | |
Schott N-SF8 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 1.03 W/m-K | 7.15 BTU-in/hr-ft²-°F | |
Arlon TC350 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |