Polymer Property : Thermal Conductivity = 7.78 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 7.78 W/m-K

@Temperature 600 °C
54.0 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Zircar Refractory Composites RS-DR Refractory Sheet
TYPE RS-DR is a rigid pre-fired sheet that has been heat-treated to remove all organic binder and is stable to moisture attack. Refractory Sheet Type RS-DR is suited for use as a setter or barrier f..