Thermal Properties Metric English Comments
Thermal Conductivity 10.5 W/m-K
72.9 BTU-in/hr-ft²-°F
HP Alloys Alloy C-276, 10% Cold Worked
10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Thermal Conductivity 10.5 W/m-K
72.9 BTU-in/hr-ft²-°F
HP Alloys Alloy C-276, 20% Cold Worked
20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Thermal Conductivity 10.5 W/m-K
72.9 BTU-in/hr-ft²-°F
HP Alloys Alloy C-276, 40% Cold Worked
40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Thermal Conductivity 10.5 W/m-K
72.9 BTU-in/hr-ft²-°F
HP Alloys Alloy C-276, 50% Cold Worked
50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Thermal Conductivity 10.5 W/m-K
72.9 BTU-in/hr-ft²-°F
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â..
Thermal Conductivity 10.5 - 10.8 W/m-K
72.9 - 75.0 BTU-in/hr-ft²-°F
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92)
Terfenol-D is the commercial name for Tb0.3Dy0.7Fe1.92; a composition of material that exhibits giant magnetostriction.Magnetostriction is the phenomenon in which an applied magnetic field causes an..
Thermal Conductivity 10.5 W/m-K
72.9 BTU-in/hr-ft²-°F
HP Alloys Alloy C-276, 30% Cold Worked
30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..