Thermal Conductivity 1.17 W/m-K

@Temperature 50.0 °C
8.12 BTU-in/hr-ft²-°F

@Temperature 122 °F
Advanced Ceramics ZEMAT® ACL 2090 - Zero Expansion Glass-Ceramic
“Zero Expansion” glass-ceramic is a transparent material now in production for applications requiring ultra-low thermal expansion. The primary crystal phase is a s-eucryptite (Li2OAl2O32SiO2) soli..