Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 11.72 W/m-K | 81.34 BTU-in/hr-ft²-°F | |
Special Metals NIMONIC® Alloy PE16 A precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. It has good strength and oxidation resistance at temperatures to about 1380°.. |