Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 93.0 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 13.4 W/m-K

@Temperature 200 °C
93.0 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 13.4 W/m-K

@Temperature 200 °C
93.0 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 13.4 W/m-K

@Temperature 200 °C
93.0 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 13.4 W/m-K

@Temperature 200 °C
93.0 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 13.4 W/m-K

@Temperature 200 °C
93.0 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 13.4 W/m-K

@Temperature 200 °C
93.0 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 13.4 W/m-K

@Temperature 200 °C
93.0 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 13.4 W/m-K
93.0 BTU-in/hr-ft²-°F
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
Information provided by Goodfellow.
Thermal Conductivity 13.4 W/m-K
93.0 BTU-in/hr-ft²-°F
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material
Product Introduction: Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC t..
Thermal Conductivity 13.4 W/m-K

@Temperature 200 °C
93.0 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..