Maximum Service Temperature, Inert 210 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
410 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets
Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc..
Maximum Service Temperature, Inert 210 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
410 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Tubes
Description: Used in mechanical, electrical and electronic applications at elevated temperatures. Retains good electrical properties at high temperatures. Self-extinguishing. Low dielectric loss fac..