Polymer Property : Maximum Service Temperature, Inert = 2401 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 1316 °C
2401 °F
from -188°C to 1316°C at 10<sup>-14</sup> Torr
BryCoat WS2 Tungsten Disulfide Coating
WS2's unique, extensively modified lamellar composition of tungsten disulfide results in a high performance dry coating lubricant. A pressurized air application processes impinges a dry metallic co..