Maximum Service Temperature, Inert 1450 °C
2640 °F
CeramTec Rubalit® A 1896 Alumina
Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele..